Clay Decorative Magnets: Working With Shrinkage Instead of Against It
Share
Why Clay Magnets Change Size Before They Ever Reach the Fridge
You roll a neat disc of clay, stamp a pattern, cut a tidy circle, and set it aside. A day or two later the same disc looks smaller and slightly cupped, and the pattern has tightened. Nothing has gone wrong. Clay loses water as it dries, and the particles pack closer together, so every dimension you cut shrinks. For decorative magnets, that change is small in absolute terms but very visible on a small object: a few millimetres of pull-in can distort a face, curl an edge, or make a pressed motif look crowded. Understanding drying shrinkage is what lets you plan the size, thickness and attachment of a magnet so the finished piece looks deliberate.
The practical move is to treat shrinkage as a design parameter. Decide what finished magnet you want, work out how much larger the wet piece needs to be, and choose a clay and construction that tolerate the change. This is not a chemistry lesson; it is the difference between a set of magnets that sit flat and look crisp and a batch that has to be re-made.
Reading the Shrinkage of Your Actual Clay
Different clays shrink by different amounts. Air-dry clay, polymer clay and various earthenware bodies are not interchangeable, and within each family the maker's data matters. Most clay manufacturers publish a shrinkage figure, often as a percentage measured from the wet or plastic state to the dry state, and sometimes a second figure for fired work. Use the figure for the clay you actually have, from its own packaging or technical sheet. Do not assume a universal number, and do not assume that two clays labelled the same way shrink identically.
If you are making air-dry clay magnets that will never be fired, you mainly care about drying shrinkage. If you are working in a fired clay body, the total change includes drying plus firing, and the maker's combined figure is the one to plan with. For a decorative magnet, the difference between, say, a modest and a larger shrinkage is easiest to handle at the design stage, when you can simply cut the blank bigger.
A simple sizing method
- Decide the diameter or length you want the finished magnet to be.
- Look up the shrinkage percentage stated for your clay.
- Divide the finished size by one minus the shrinkage fraction to estimate the wet size, then add a small margin for trimming and for the unevenness of hand-cutting.
- Make one or two test pieces from the same batch, let them dry fully, and measure them before committing to a whole set.
The test piece is the honest check. A single trial disc dried on the same surface you plan to use tells you more about your own clay, thickness and drying conditions than any table. Keep the trial piece alongside the real batch so both experience the same conditions.
Drying Changes Shape as Well as Size
Shrinkage is rarely uniform in a small, hand-formed object. Thicker areas hold more water and release it more slowly than thin edges. If one part of a magnet dries faster than another, the slower part lags behind, and the object can warp, cup or crack. On a flat disc, the rim often dries first and pulls inward, while the centre stays damp and resists, which is a common route to a curled edge.
Two features of magnet-making amplify this. First, magnets are usually thin, so there is little body to resist distortion. Second, the surface is often decorated with texture, impressions or applied pieces, which create thickness differences. A stamped motif compresses clay and changes how that area dries. Applied dots, petals or letters sit proud of the base and dry at a different rate from the slab beneath them.
The response is to keep the object as even in thickness as you can, dry it slowly and evenly, and avoid laying it on a surface that grips. A non-stick board, a sheet of baking parchment or a lightly dusted tile lets the piece slide slightly as it contracts instead of being held fast. Turning the piece over partway through drying, when it is firm enough to handle without deforming, helps both faces dry at a similar rate. Covering the work loosely for the first stage slows surface drying and gives the interior time to catch up.
Design choices that suit shrinkage
- Simple silhouettes: circles, ovals and rounded rectangles distribute stress better than thin, spiky shapes with narrow necks.
- Even thickness: roll the slab to a consistent thickness, and keep applied decoration low and well pressed down.
- Texture with rounded edges: deep, sharp impressions concentrate stress; shallow, rounded stamps are more forgiving.
- Small overhangs: avoid unsupported protruding parts that can sag as the clay softens and pulls.
These are design preferences, not rules. A delicate shape can work if you dry it slowly and support it, but it needs more attention than a plain disc.
Matching the Magnet to the Finished Clay Piece
Shrinkage affects the back of the magnet as much as the front. The magnet you attach must sit flat on a surface that is now smaller and possibly slightly curved. Plan the attachment for the dry dimensions, not the wet ones, and leave a clear margin around the magnet so no adhesive squeezes out at the edge.
For a small decorative magnet, a thin disc or a small rectangular magnet is usually enough to hold a note or a photo. The magnet's own stated pull and size are the figures to work from; a decorative object is not a load-bearing fixing, and the magnet should be sized so the finished piece is easy to lift off the fridge without the clay flexing. Stronger, larger magnets are easy to over-specify on a thin clay body: the snap of removal can stress the bond or crack a brittle piece. Match the magnet to the weight and thickness of the finished object, and if in doubt, test one piece before making a set.
Adhesion matters more than raw magnet strength. Many craft magnets come with a self-adhesive backing, which works best on a clean, dry, flat surface. For a porous or dusty clay back, a small amount of a suitable craft adhesive applied to a roughened area gives a more dependable hold than a peel-and-stick pad alone. Let the adhesive reach full strength before the magnet is used. The point is not to build a heavy-duty fixing; it is to make a light decorative object that stays put and comes away cleanly.
Finishing a Shrunken, Dried Piece
Once the piece is fully dry, check it for flatness before you decorate further. A dried clay magnet that rocks on the fridge is usually a drying problem, not an adhesive problem, and no magnet will make a warped back sit flat. If a piece has cupped, you can sometimes correct a slight curve by placing it face down on a flat surface and applying gentle, even weight while it finishes drying, but badly warped pieces are better re-made with slower drying.
Dried clay is dusty. Wipe the back with a dry cloth or a lightly damp one and let it dry completely before applying adhesive. Finish the face with a compatible paint, glaze or sealant according to the product's own instructions. Drying and curing are separate stages: paint that is dry to the touch may not be cured, and a sealed surface may need longer before the magnet is handled. Follow the product's stated schedule rather than guessing.
If you are firing the clay, the maker's firing schedule and the behaviour of the body govern the process, and the final size is only known after firing. For decorative magnets, a fired, glazed finish gives a durable, wipeable face, but the extra steps and the second shrinkage stage mean you should plan the whole batch around the maker's combined figures.
Building a Consistent Set
Shrinkage is easiest to manage when you work in batches. Roll one slab at a consistent thickness, cut all the blanks at once, and dry them together under the same cover. That way the pieces shrink by similar amounts and still look like a set. If you cut some pieces on day one and others on day three, the later pieces are already drying differently and the final sizes drift apart.
Keep a simple record: the clay used, the wet size you cut, the date, and the dry size measured later. After one or two batches you have your own working figure for that clay and your own conditions, which is more useful than a generic percentage. The same record helps you reorder materials: you will know how much clay a dozen magnets takes, and whether your slab thickness leaves the pieces robust enough to handle.
Useful supplies for this kind of work are modest: a smooth rolling surface and a pair of thickness guides for even slabs, a non-stick board or parchment for drying, a set of shallow texture tools or stamps, and small craft magnets with a suitable adhesive. The value is not in owning many tools; it is in choosing a few that keep thickness even and drying controlled. A consistent slab and a slow, covered dry are what turn a fragile wet disc into a reliable finished magnet.
The satisfying result is a set of small, flat, crisply decorated magnets that look the same as the day they were planned, because the shrinkage was allowed for rather than discovered afterwards. Work out the clay's behaviour, cut with the finished size in mind, dry evenly, and match the magnet to the dried piece. The material will still move; the design simply makes that movement part of the plan.